Welding Technology - Welding Defects Collection (2)
2019-10-08
10. Wagon Track Slag Line
11. Interrun Fusion
12. Lack of Side Wall Fusion
13. Porosity
14. Cluster Porosity
15. Hollow Bead
16. Transverse Crack
17. Center Line Crack
18. Root Crack